--- /dev/null
+Arrive 9:30am
+
+- Curves have changed as before overnight
+ - Maybe the act of evaporating "resets" the curve?
+ - Try turning the sample holder around, wait ~1hour, turn back and see if curve changes
+ - Control, before turning around: 101738.dat
+ - Now we play the waiting game
+ - Turn around at 112621.dat
+ - Curves appear very similar
+ => Conclude that the change in curve is due to the deposition of the Au layers
+
+ - Try deposition of more Au
+ - This time increase current. Previous depositions are too slow. 4.6A not enough?
+ - Odd, because normally 3.5A is enough to be able to visibly see deposition after ~30min
+ - The Au ball is not on the apex of the Tungsten wire; it is not receiving as much heat
+ - Hopefully increasing the current will not destroy the filament